Wednesday, November 25, 2026

GMAW (MIG) "strength is all in the bead on the surface"

  That is the generally accepted wisdom, and it's what the welding engineer who taught my MIG classes taught, and I believe it to this day.  It is because MIG isn't known for great penetration.

BUT THAT'S OKAY.


 Here we have some 1/8in + CRS plate which I welded to a piece of 1/2in rebar in the flat position.  Length is roughly 4 in.

 You can probably tell that penetration was around 50% (and highly variable because I am not a welder)

Here is the bead side.  Bead doesn't even seem to be halfway onto the rebar, TBH, more of it is on the plate.  If I were doing something to sell, I would weld the other side too.

 But here's the thing: I did this as an unscientific coupon test.  I put it in the big bench vise, and beat the living tarmuck out of it with a five pound sledge hammer.  I was destroying everying attached to my workbench with the hammer blows, but that steel did not yield (much).  I hit it many times in both directions.  After the third round I gave up and left it in latest semi-bent position.  I didn't straighten it.  This pics were taken after that.  You can see it is not bent much.

 So despite poor penetration, that bead produced a serviceable weld.  And oh dear, I failed to produce the celebrated "stacked dimes" appearance, because pretty isn't as important as strength.


 ~≈{👁}≈~